In this work, the influence of microwave drying parameters such as irradiation time and microwave power level on the properties of synthetic moulding sands is presented. Determination of compressive strength Rc s, shear strength Rt s and permeability Ps of synthetic moulding sands with the addition of two different bentonites, after drying process with variable microwave parameters were made. The research works were carried out using the microwave oven with regulated power range of the electromagnetic field. From the results obtained, the significant influence of both drying time and microwave power level on the selected properties of moulding sands was observed. In comparison to the conventional drying method, microwave drying allows to obtain higher compressive strength of the synthetic moulding sand. The influence of application microwave irradiation on permeability was not observed. Higher strength characteristics and shorter drying time are major advantages of application of the electromagnetic irradiation for drying of the synthetic moulding sand with regard to conventional drying method.
Go to article

Abstract

Ablation casting is a technological process in which the increased cooling rate causes microstructure refinement, resulting in improved mechanical properties of the final product. This technology is particularly suitable for the manufacture of castings with intricate shapes and thin walls. Currently, the ablation casting process is not used in the Polish industry. This article presents the results of strength tests carried out on moulding sands based on hydrated sodium silicate hardened in the Floster S technology, intended for ablation casting of the AlSi7Mg (AK7) aluminium alloy. When testing the bending and tensile strengths of sands, parameters such as binder and hardener content were taken into account. The sand mixtures were tested after 24h hardening at room temperature. The next stage of the study describes the course of the ablation casting process, starting with the manufacture of foundry mould from the selected moulding mixture and ending in tests carried out on the ready casting to check the surface quality, structure and mechanical properties. The results were compared with the parallel results obtained on a casting gravity poured into the sand mould and solidifying in a traditional way at ambient temperature.
Go to article

Abstract

Moulding properties of Isasa River Sand bonded with Ipetumodu clay (Ife-North Local Government Area, Osun State, Nigeria) were investigated. American Foundry men Society (AFS) standard cylindrical specimens 50mm diameter and 50mm in height were prepared from various sand and clay ratios (between 18% and 32%) with 15% water content. The stress-strain curves were generated from a universal strength testing machine. A flow factor was calculated from the inclination of the falling slope beyond the maximum compressive strength. The result shows that the flowability of the samples increases from 18% to 26% clay content, its maximum value was attained at 26% and then it decreases from 30% to 32% clay content. The green compressive strength, dry compressive strength and air permeability values obtained from the mould samples were in accordance with standard values used in foundry practice. The x-ray diffraction test shows that the sand contains silicon oxide (SiO2), Aluminium oxide (Al2O3), and Aluminium silicate (Al6Si2O13). The mould samples were heated to a temperature of 1200 o C to determine the sintering temperature; fussion did not take place at this temperature. The results showed that the sand and clay mixture can be used to cast ferrous and non-ferrous alloys.
Go to article

Abstract

Until now, the mould sand in general use in the foundry industry are based on bentonite, which resulted from the fact that a good recognition properties and phenomena associated with this material. Come to know and normalized content of montmorillonite and carbonates and their important role in the construction of bentonite, and mass properties of the participation of compressive strength or scatter. Halloysite is widely used in industry and beyond them. However, little is known about its use in the foundry in Poland and abroad. This article presents preliminary research conducted at the Foundry Department of Silesian University of Technology on this material. Will raise the question of the representation of this two materials, which contains information connected with history and formation of materials, their structure and chemical composition. In the research, the results of compressive strength tests in wet masses of quartz matrix, where as a binder is used halloysite and bentonite in different proportions.
Go to article

Abstract

The aim of the study was to determine the applicability of a new product added to water glass-containing foundry sands hardened with ethylene glycol diacetate. The new additive designated by the symbol "B" is a composition of aqueous solutions of modified polyalcohols, improving the sand knocking out properties. The scope of studies included testing various mechanical and technological properties of foundry sand mixtures, such as permeability, friability, life cycle of cores and knocking out properties. In the technological studies, two types of water glass with different values of the silica modulus and density, designated as R145 and R150, were used. Moulding sands were prepared with the additive "B". For comparison, reference sands with water glass but without the additive "B" were also made. In Part I of the article, the results of studies of the effect of additive "B" on the properties of foundry sands with water glass hardened by CO2 blowing were discussed.
Go to article

Abstract

Modern investigation methods and equipment for the quality estimation of the moulding sands matrices with organic binders, in their circulation process, are presented in the paper. These methods, utilising the special equipment combined with the authors investigation methods developed in the Faculty of Foundry Engineering, AGH the University of Science and Technology, allow for the better estimation of the matrix quality. Moulding sands systems with organic binders require an in-depth approach to factors deciding on the matrix technological suitability as well as on their environmental impact. Into modern methods allowing for the better assessment of the matrix quality belongs the grain size analysis of the reclaimed material performed by means of the laser diffraction and also the estimation of the moulding sand gas evolution rate and identification of the emitted gases and their BTEX group gases content, since they are specially hazardous from the point of view of the Occupational Safety and Health.
Go to article

Abstract

Using the available analytical methods, including the determination of chemical composition using wavelength-dispersive X-ray fluorescent spectroscopy technique and phase composition determined using X-ray diffraction, microstructural observations in a highresolution scanning microscope equipped with an X-ray microanalysis system as well as determination of characteristic softening and sintering temperatures using high-temperature microscope, the properties of particular chromite sands were defined. For the study has been typed reference sand with chemical properties, physical and thermal, treated as standard, and the sands of the regeneration process and the grinding process. Using these kinds of sand in foundries resulted in the occurrence of the phenomenon of the molding mass sintering. Impurities were identified and causes of sintering of a moulding sand based on chromite sand were characterized. Next, research methods enabling a quick evaluation of chromite sand suitability for use in the preparation of moulding sands were selected.
Go to article

Abstract

The aim of the hereby paper is to present the developed model of determining the volume and surface porosity based on the main fraction of polifractional materials, its experimental verification and utilisation for the interpretation of effects accompanying the formation of a moulding sand apparent density, porosity and permeability in the blowing processes of the core and moulds technology.
Go to article

Abstract

The cumulative results of investigations of the possibility of using the reclaimed materials after the mechanical, thermal or mechanical-thermal reclamation for making cores by means of the blowing method in the alkaline CO2 technology, are presented in the paper. Three kinds of spent sands: with furfuryl resin, bentonite and alkaline phenolic resin, obtained from the foundry, were subjected to three kinds of reclamation: mechanical, thermal and combined mechanical-thermal, applying for this aim adequate experimental devices. The obtained reclaims were assessed with regard to the degree of the matrix liberation from the determined binding material. Reclaims of moulding sands with binders of the form of resin were assessed with regard to ignition loss values and pH reaction, while reclaims of moulding sands with bentonite with regard to the residual clay content and pH value. In all cases the results of the performed sieve analyses were estimated and the average characteristic diameter dl was determined. The reclaimed matrix was applied as a full substitute of the fresh high-silica sand in typical procedures of preparing core sands used for making shaped samples for bending strength investigations, Rg u .
Go to article

Abstract

The paper presents results of preliminary examinations on possibility of determining binder content in traditional moulding sands with the microwave method. The presented measurements were carried-out using a special stand, the so-called slot line. Binder content in thesandmix was determined by measurements of absorption damping Ad and insertion losses IL of electromagnetic wave. One of main advantages of the suggested new method of binder content measurement is short measuring time.
Go to article

Abstract

It was found that the addition of carbon fibers (CFs) does not affect the crosslinking process in the microwave radiation (800 W, 2.45 GHz) of the BioCo2 binder, which is a water solution of poly(acrylic acid) and dextrin (PAA/D). It has influence on BioCo2 thermal properties. The CFs addition improves the thermostability of a binder and leads to the reduction of gas products quantity generated in the temperature range of 300-1100°C (TG-DTG, Py-GC/MS). Moreover, it causes the emission of harmful decomposition products such as benzene, toluene, xylene and styrene to be registered in a higher temperatures (above 700°C). BioCo2 binder without CFs addition is characterized by the emission of these substances in the lower temperature range. This indicates the positive effect of carbon fibers presence on the amount of released harmful products. The selected technological tests (permeability, friability, bending strength, tensile strength) have shown that the moulding sand with the 0.3 parts by weight carbon fibers addition displays the worst properties. The addition of 0.1 parts by weight of CFs is sufficient to obtain a beneficial effect on the analyzed moulding sands properties. The reduction of harmful substances at the higher temperatures can also be observed.
Go to article

Abstract

Bentonite is clay rock, which is created by decomposition of vulcanic glass. It is formed from mixture of clay minerals of smectite group, mainly montmorillonite, beidellite and nontronite. Its typical characteristics is, that when in contact with water, it intensively swells. First who used this term was W.C. Knight in 1887. The rock had been named after town Fort Benton in American state Montana. For its interesting technological properties and whiteness has wide technological use. Bentonite is selectively mined and according to its final use separately modified, which results in high quality product with specific parameters. In the beginning of 21st century belong bentonite moulding mixtures in foundry to always perspective. Mainly increased ratio of ductile cast iron castings production cannot be ensured without the need of quality bentonite. Great area of scope remains to further research of moulding materials, which return also to bentonite producers.
Go to article

Abstract

Casting quality depends on many factors including the quality of the input materials, technology, material securing and last but not least, the mould into which the casting is casted. By pouring into a single-shot mould, based mainly on 1st generation binders, is is a very important factor. Basically, a bentonite mixture represents either a three- or four-component system, but each component of the system is a heterogeneous substance. This heterogeneity punctuates mainly a non-stationary heat field, presented throughout the whole process of the casting production. The most important component is a binder and in the case of first generation binders mostly bentonites are used - clays that contain minimum of 80% of montmorillonite
Go to article

Abstract

The paper presents the results of laboratory tests into the effects of moisture and the content of two types of bentonite on dielectric properties of moulding sand. The use of electromagnetic waves in foundry industry is becoming more and more popular, which provides to some extent alternatives to conventional drying methods. Experimental studies published so far have shown the validity of using microwaves for drying classic moulding sands with bentonite. However, these studies lack data on the effect of moisture or bentonite content in moulding sand on the real component ε' or imaginary component ε'' of the relative complex electrical permittivity. The presented results may become in the future the basis for the evaluation of the composition of moulding sands, taking into account the phenomena occurring under the influence of electromagnetic field, which directly translates into the quality of the castings made and may constitute an attempt to develop a mathematical model of electric properties of moulding sands.
Go to article

Abstract

Substituting of ethyl silicate with ecologic sols of colloidal silica in the investment casting technology, resulting from the increased demands concerning environmental protection, caused the prolongation of production cycle for precision castings produced in multi-layer thin-walled ceramic shell moulds. Modification of Sizol 030 binder with benzoyl peroxide, proposed in the paper, was aimed at restriction of time needed for realization of a single layer of the shell mould, and by the same, of such a mould as a whole. Examination of kinetics of the drying process were held for the layers made of prepared moulding material and the influence of binder modification on the mould curing time was determined.
Go to article

Abstract

The paper presents measurement results of standing wave ratio to be used as an efficiency indicator of microwave absorption by used moulding and core sands chosen for the microwave utilization process. The absorption measurements were made using a prototype stand of microwave slot line. Examined were five used moulding and core sands. It was demonstrated that the microwave absorption measurements can make grounds for actual microwave utilization of moulding and core sands.
Go to article

Abstract

The new investigation method of the kinetics of the gas emission from moulding sands used for moulds and cores is presented in this paper. The gas evolution rate is presented not only as a function of heating time but also as a function of instantaneous temperatures. In relation to the time and heating temperature the oxygen and hydrogen contents in evolving gases was also measured. This method was developed in the Laboratory of Foundry Moulds Technology, Faculty of Foundry Engineering, AGH. Gas amounts which are emitted from the moulding sand at the given temperature recalculated to the time unit (kinetics) are obtained in investigations. Results of investigations of moulding sand with furan resin are presented - as an example - in the paper.
Go to article

Abstract

Gas emission from casting moulds, cores and coatings applied for sand and permanent moulds is one of the fundamental reasons of casting defects occurrence. In the previous studies, gas emission was measured in two ways: normalized, in which the evolving gas volume was measured during heating of the moulding sand sample in a sealed flask, or by measuring the amount of gas from sand core (sample) which is produced during the pouring of liquid metal. After the pouring process the sand mould is heated very unequally, the most heated areas are layers adjacent to the liquid metal. The emission of gas is significantly larger from the surface layer than from the remaining ones. New, original method of measuring kinetics of gas emission from very thin layers of sand moulds heated by liquid metal developed by the authors is presented in the hereby paper. Description of this new method and the investigation results of kinetics of gas emission from moulding sand with furan and alkyd resin are shown. Liquid grey cast iron and Al-Si alloy were used as a heat source in the sand moulds. Comparison of the kinetics of gas emission of these two kinds of moulding sands filled with two different alloys was made. The momentary metal temperature in sand mould was assigned to the kinetics of gas emission, what creates a full view of the possibility of formation of casting defects of the gaseous origin. Moulding sand with alkyd resin is characterized by larger gas emission; however gases are emitted slower than in the case of moulding sands with furan resin. This new investigation method has a high repeatability and is the only one which gives a full view of phenomenon’s in the surface layer which determines quality of the casings. The obtained results are presented on several graphs and analyzed in detail. They have a great application value and can be used in the production of iron as well as light metal alloy castings.
Go to article

Abstract

The paper presents the results of an investigation of the thermal deformation of moulding sands with an inorganic (geopolymer) binder with a relaxation additive, whose main task is to reduce the final (residual) strength and improves knocking-out properties of moulding sand. The moulding sand without a relaxation additive was the reference point. The research was carried out using the hot-distortion method (DMA apparatus from Multiserw-Morek). The results were combined with linear deformation studies with determination of the linear expansion factor (Netzsch DIL 402C dilatometer). The study showed that the introduction of relaxation additive has a positive effect on the thermal stability of moulding sand by limiting the measured deformation value, in relation to the moulding sand without additive. In addition, a relaxation additive slightly changes the course of the dilatometric curve. Change in the linear dimension of the moulding sand sample with the relaxation additive differs by only 0.05%, in comparison to the moulding sand without additive.
Go to article

Abstract

The effects of silica additive (Poraver) on selected properties of BioCo3 binder in form of an aqueous poly(sodium acrylate) and dextrin (PAANa/D) binder were determined. Based on the results of the thermoanalytical studies (TG-DTG, FTIR, Py-GC/MS), it was found that the silica additive results in the increase of the thermostability of the BioCo3 binder and its contribution does not affect the increase in the level of emissions of organic destruction products. Compounds from group of aromatic hydrocarbons are only generated in the third set temperature range (420-838°C). The addition of silicate into the moulding sand with BioCo3 causes also the formation of a hydrogen bonds network with its share in the microwave radiation field and they are mainly responsible for maintaining the cross-linked structures in the mineral matrix system. As a consequence, the microwave curing process in the presence of Poraver leads to improved strength properties of the moulding sand (���� �� ). The addition of Poraver's silica to moulding sand did not alter the permeability of the moulding sand samples, and consequently reduced their friability. Microstructure investigations (SEM) of microwave-cured samples have confirmed that heterogeneous sand grains are bonded to one another through a binder film (bridges).
Go to article

Abstract

In the paper, a research on effects of baking temperature on chromite sand base of moulding sands bonded with sodium silicate is presented. Pure chromite sand and its chromite-based moulding sand prepared with use of sodium silicate were subjected to heating within 100 to 1200 °C. After cooling-down, changes of base grains under thermal action were determined. Chromite moulding sand was prepared with use of 0.5 wt% of domestic made, unmodified sodium silicate (water-glass) grade 145. After baking at elevated temperatures, creation of rough layer was observed on grain surfaces, of both pure chromite sand and that used as base of a moulding sand. Changes of sand grains were evaluated by scanning microscopy and EDS analyses. It was found that changes on grain surfaces are of laminar nature. The observed layer is composed of iron oxide (II) that is one of main structural components of chromite sand. In order to identify changes in internal structure of chromite sand grains, polished sections were prepared of moulding sand hardened with microwaves and baked at elevated temperatures. Microscopic observations revealed changes in grains structure in form of characteristically crystallised acicular particles with limited magnesium content, intersecting at various angles. EDS analysis showed that these particles are composed mostly of chromium oxide (III) and iron oxide (II). The temperature above that the a.m. changes are observed in both chromite-based moulding sand and in pure chromite sand. The observed phenomena were linked with hardness values and mass of this sand.
Go to article

Abstract

Emission of gases under high temperature after pouring molten metal into moulds, which contain the organic binder or other additives (solvents or curing agent), may be an important factor influencing both on the quality of the produced castings, and on the state of environment. Therefore, a comprehensive study of the emitted gases would allow to determine restrictions on the use of the moulding sands in foundry technologies, eg. the probability of occurrence of casting defects, and identify the gaseous pollutants emitted to the environment. The aim of the research presented in this paper was to determine the amount of gases that are released at high temperatures from moulding sands bonded by biopolymer binder and the quantitative assessment of the emitted pollutants with particular emphasis on chemical compounds: benzene, toluene, ethylbenzene and xylenes (BTEX). The water-soluble modified potato starch as a sodium carboxymethyl starch with low (CMS-NaL) or high (CMS-NaH) degree of substitution was a binder in the tested moulding sands. A tests of gases emission level were conducted per the procedure developed at the Faculty of Foundry Engineering (AGH University of Science and Technology) involving gas chromatography method (GC). The obtained results of the determination of amount of BTEX compounds generated during the decomposition process of starch binders showed lower emission of aromatic hydrocarbons in comparison with binder based on resin Kaltharz U404 with the acidic curing agent commonly used in the foundries.
Go to article

Abstract

This paper focuses on mechanical properties of self hardening moulding sands with furfuryl and alkyd binders. Elasticity as a new parameter of moulding sands is investigated. With the use of presented testing equipment, it is possible to determine force kinetics and deformation of moulding sand in real time. The need for this kind of study comes from the modern casting industry. New foundries can be characterized with high intensity of production which is correlated with high level of mechanization and automatization of foundry processes. The increasingly common use of manipulators in production of moulds and cores can lead to generation of new types of flaws, caused by breakage in moulds and cores which could occur during mould assembly. Hence it is required that moulds and cores have high resistance to those kinds of factors, attributing it with the phenomenon of elasticity. The article describes the theoretical basis of this property, presents methods of measuring and continues earlier research.
Go to article

Abstract

The problem related to the management of post reclamation dusts generated in the reclamation process of waste moulding sands with organic binders is presented in the hereby paper. Waste materials generated in this process are products hazardous for the environment and should be utilised. The prototype stand for the utilisation of this dangerous material in its co-burning with coal was developed and patented in AGH in Krakow. The stand was installed in one of the domestic casting houses. As the utilisation result the transformed waste product is obtained and its management in the production of ceramic materials constitutes the subject of the presented publication.
Go to article

Abstract

In the knock-out process, as well as in the preliminary phase of moulding sand reclamation, the issue of energy demand for the process of crushing used sand agglutinations, preferably to single grains, is particularly important. At present, numerical values of moulding sand impact resistance, which would allow energy-related aspects of this process to be forecast, are not known, as such research has not been carried out. It seems that impact resistance tested on very small cross-section samples, which allows us to very precisely reveal some unique features of a moulding sand with organic and inorganic binders, is an important parameter, which so far has not been taken into account for evaluation of mechanical properties of moulding sands. Preliminary attempts to determine impact resistance of moulding sands have been carried out as part of own research of the author. The conducted investigations aimed at determining the relationships between the obtained values of tensile strength and impact resistance of moulding sands. In addition, the effect of holding samples at temperatures of 100oC, 200oC, 300oC on the value of impact resistance was determined, both for sands made with fresh and with reclaimed sand grains.